Alloyed fine powder
Achieving micron-order alloy fine powder
Kobe Steel's alloyed fine powder is manufactured using a high pressure water atomization method and is used for metal powder injection compacting (MIM) in many cutting edge industries including electronics and latest machineries.

Features
- Average particle size of around 10 μm
- Minimal segregation of alloy components
Particle Size Distribution

Chemical Composition
Steel grade name | Specifications | C | Si | Mn | P | S | Ni | Cr | Mo | V | Cu | Nb |
---|---|---|---|---|---|---|---|---|---|---|---|---|
FA-SUS304L | Min Max |
0.03 | 1.00 | 2.00 | 0.045 | 0.030 | 9.00 13.00 |
18.00 20.00 |
||||
FA-SUS316L | Min Max |
0.08 | 1.00 | 2.00 | 0.045 | 0.030 | 10.00 14.00 |
16.00 18.00 |
2.00 3.00 |
|||
FA-SUS430 | Min Max |
0.12 | 0.75 | 1.00 | 0.040 | 0.030 | 16.00 18.00 |
|||||
FA-SUS440C | Min Max |
0.95 1.20 |
1.00 | 1.00 | 0.040 | 0.030 | 0.60 | 16.00 18.00 |
0.75 | |||
FA-SUS630 | Min Max |
0.07 | 1.00 | 1.00 | 0.040 | 0.030 | 3.00 5.00 |
15.00 17.00 |
3.00 5.00 |
0.15 0.45 |
||
FA-SKD11 | Min Max |
1.40 1.60 |
0.40 | 0.60 | 0.030 | 0.030 | 11.00 13.00 |
0.80 1.20 |
0.20 0.50 |
Upon request materials other than the above can also be supplied.